Additive manufacturing turns a STEP file into a part in days — and stops paying when the batch grows.
What comes in: a STEP file, a quantity, the duty (temperature, load, contact media), the tolerances that must hold, and the finishing. That is the whole input. Nothing else is needed to start a review.
What comes back: a written DFM note in 24–48 hours naming the machine, the build orientation, the tolerance class and the finishing route — then parts from four build envelopes, up to 1200 × 800 × 1000 mm per part, in 24 grades across nine families.
The condition: additive is a low-volume route. Its per-part price is nearly flat with quantity, and that is exactly why it loses to a tool at volume. We say where that crossover sits before the quotation, not after the invoice.
FDM melts a thermoplastic and lays it down one bead at a time. Everything below follows from that.
Filament is fed into a nozzle, melted, and laid along a tool path as a bead. The bead fuses to the one beside it and to the layer underneath while both are still hot, then cools and sets. Nothing is cast in one shot and nothing is cut out of a block: the part is built from the bed up, layer on layer, and every layer is a weld.
The layer boundary is a weld, not a glue line.
Two hot surfaces in contact swap polymer chains across the interface and set as one piece. How strong that interface ends up depends on how hot the two surfaces were and how long they stayed that way — which is why the chamber is held at temperature instead of left open. It is a real bond. It is simply not as strong as the material inside the bead.
So the layer boundary is the ceiling on strength.
In the plane of a layer a part carries close to the bulk properties of its grade. Across layers it carries less, and it fails by peeling one layer off the next. That is a property of the process, not a defect in your part: every FDM part has it, and no setting removes it. Design the load path in-plane and it stops mattering. Ignore it and it decides where the part breaks.
Which makes orientation a design decision, not a setup step.
Rotate the same part and a load that ran in-plane now runs across layers. Orientation also moves the support footprint, the finish each face ends up with, and the shrinkage direction. We fix it at DFM and print it in the note, because a strength call without an orientation is only half a call.
Why that suits functional parts, and rules it out for appearance parts.
A part with a job can be designed around the layers.
You know which way the load runs, so the part is oriented to carry it in-plane. The grades are the polymer families moulded parts already use — PA, PC, ABS, PPS, PPA, PEEK — so a printed trial is a real material trial, not a stand-in. The geometry rules are stated before the build rather than discovered in it: structural walls from 0.8 mm, threads from M3, anything finer goes to a tapped hole or a heat-set insert.
A part that has to look like something is a different question.
Layer texture follows layer height and surface angle. On a vertical wall it reads as fine; on a sloped or curved face the stair-step is the geometry and it cannot be tuned away. Layer height runs 0.10–0.30 mm, and 0.10 mm only moves the steps closer together. Where a Class-A face is specified, the part is printed oversize and machined, or it is moulded.
What we do not claim: a strength figure for the layer boundary. It moves with the grade, the chamber temperature, the orientation and the bead overlap, so one number would describe one build and not yours. Where a joint has to carry load across layers, it is tested on the first article or the geometry is changed.
Twenty-four grades in nine families. Pick by the duty, not by the name.
A grade is a compromise, not an upgrade. Carbon fibre buys stiffness and is paid for in elongation; flame retardant buys a rating and is paid for in surface; high performance buys heat resistance and is paid for in price. Each family below is listed with the duty it does not fit, because that is the half of the choice that gets skipped.
Family and grades
What it solves
Choose it when
Do not choose it when
Engineering basics PETG · PAHT · ABS+ · PC
General structural and cosmetic parts; lowest unit price. HDT 50–111 °C across the four.
Housings, brackets, jigs, spacers — no extreme heat or chemical duty.
Duty above PC's 111 °C; a UL94, ESD or flex requirement.
Stiffness. Tensile to 93 MPa, flexural to 144 MPa. Elongation 1.5–6.5 %.
Load-bearing brackets, jigs, end effectors, drone frames — where deflection is the limit.
The part has to bend or take impact; a cosmetic face is specified; UL94 or ESD is required.
Glass fibre GF PAHT-GF · PC-GF · PET-GF
Stiffness and heat resistance below carbon's price. HDT 77–109 °C.
Load-bearing parts with a moderate duty; insulating and wear parts.
You need the highest stiffness per gram; a cosmetic face is specified; UL94 or ESD is required.
Flame retardant FR PC/ABS-FR
A UL94 route. The rating and the thickness have to be named; a material name is not a report.
Thin-wall housings, power supply and connector bodies, brackets inside an enclosure.
No rating or thickness is given; vapour smoothing is on the route — the FR grade goes white under it; the duty is multi-year outdoor.
Anti-static ESD PETG-ESD
A surface resistance inside a stated range. Give the range first, then the grade.
Trays, racks, PCB handling fixtures, test jigs, packaging inserts.
No resistance range is given; the part runs hot (HDT 68 °C); the part carries structural load.
Elastomers TPU95A · PEBA95A
Soft, resilient, tolerant of repeated flexing. Elongation ≥800 % and ≥1000 %.
Gripper pads, vibration pads, seals, living hinges, midsoles.
The part locates, threads or holds a bearing; it runs hot (HDT 53–70 °C); a seal sits under permanent compression.
High performance PPS-CF · PPS-GF · PPA-CF · PPA-GF
Heat and chemical duty. HDT 227–264 °C; tensile to 169 MPa. Read the price with the process window.
Under-bonnet and EV parts, chemical-handling parts, connectors, ADAS sensor covers, robot arms.
The part is a fit-check sample — validate the geometry in a basic grade first; the part has to bend or take impact (elongation 1.2–2.1 %).
Specialty PEEK · PEEK-CF
Impact and corrosion resistance for extreme service — offshore, aerospace, repeated sterilisation. HDT 139–165 °C.
Re-sterilised instrument handles, aerospace brackets and heat shields, wafer-handling parts.
An ordinary room-temperature structural part; a part-level material certificate is required.
Special purpose PolyCast · OrthoTough 1000
Compounded for one operation. PolyCast replaces wax as a casting pattern; OrthoTough 1000 is tested to GB/T 16886 and ISO 10993 for skin contact.
Small-batch metal parts going through investment casting; orthoses in long-term skin contact.
Used as a general structural grade — off-purpose it performs worse than a general grade; a device-level certificate is required.
Every figure above is a typical value in the process window, taken from the grade data sheet — not a part-level guarantee. One page per grade, with the full table and the applications, sits under the material range →
Four envelopes. A part that does not fit one of them is a different part, not a larger print.
Envelope size decides whether a part comes out in one piece. Everything downstream — the machine, the orientation, the tolerance class, the date — follows from that, so it is settled in the DFM note rather than after the first build.
VULCAN 1200
1200 × 800 × 1000 mm
The largest envelope. Housings, large fixtures and one-piece structural parts: no sectioning, and no seam to re-qualify afterwards.
VULCAN 600
600 × 500 × 500 mm
The heated-chamber machine. PEEK, PPS and PPA batches run here, which is why a high-temperature grade and a large envelope are two conditions that have to be checked against each other.
SC12060
1200 × 600 × 600 mm
Long parts: rails, profiles, long brackets. Linear-motor drive, effective print speed to 500 mm/s — the reason a long part stays one build instead of three.
X2PRO
300 × 300 × 260 mm
Small parts and fine detail, many per build, lowest unit cost. Iteration rounds run here.
When the part is bigger than every envelope, three things are decided at once.
Where the seam goes.
Into the lowest-stress section, away from sealing faces, bearing seats and locating features. That is a geometry decision, so it is taken with you and not handed down with the quotation.
How the two halves join.
A keyed joint or a structural adhesive, named in the note. Both need a surface the finishing route can deliver, and a bonded joint is only as good as the face it is bonded to.
How the joint is qualified.
A seam is not the same material as the part. Where it carries load, the joint is checked on the first article against the load direction it will see. The drawing alone does not qualify it.
Size is not the only constraint. PEEK, PPS and PPA run on the heated-chamber machine, whose envelope is smaller than the largest one, so a large part that also needs one of those grades has to settle which condition gives first. That trade changes the price and the date, and it is why the machine is named before the price.
Additive buys geometry. It does not buy unit cost.
Two boundaries decide whether a part belongs on this route: what the shape can do, and how many parts you need. Both have to be answered before a process is named, because the answer to one changes the answer to the other.
Complexity is free. Volume is not.
Internal channels, undercuts, lattices, and five parts merged into one cost the same to print as a solid block of the same volume. What additive charges for is material mass and machine time, not shape. That is the one advantage a mould cannot match: a mould charges for every feature that has to be demoulded, and again for every change to it.
The crossover is a volume, not a preference.
On additive, the hundredth part costs about what the first one did. Tooling inverts that: a high one-off cost spread across the batch, so the unit price falls as the batch grows. Below the crossover there is no tool to pay for, and printing wins; above it the tool has been paid, and moulding wins. We locate that point per part, per material and per finishing route, and write it into the DFM note.
The stage matters more than the technology.
Additive belongs at design validation, at fit and function trials, on jigs and fixtures, on spares and obsolete parts, and on the bridge between a frozen design and a tool that does not exist yet. In serial production it belongs only where the geometry or the volume makes a tool uneconomic — not because it is the newer process.
The boundary against moulding and machining, stated row by row
Question
Additive
Injection moulding
CNC
Shape freedom
Any wall the nozzle can reach; internal channels and lattices built in one pass
Constant wall, draft angle, no undercut without a slider
Any wall a cutter can reach; internal channels need a split part or a second operation
What sets the unit price
Material mass and machine hours; shape is nearly free
Tool cost amortised over the batch, so the unit price falls with quantity
Setup and programming per part, so the unit price falls slowly
Surface as delivered
Layer texture on sloped and curved faces; cosmetic faces need blasting or polishing
Tool finish, textured or polished, repeated exactly
Tool marks; roughness set by the finishing pass
Material choice
Thermoplastics in 24 grades; metals through a partner line
Any mouldable grade, at a minimum order that pays for the tool
Any machinable grade, metals included
Cost of a revision
A new file and a new build
Usually a tool modification
A new program
What we do not claim: additive does not beat a mould that is already paid for, and it does not become cheaper with volume. Where CNC, moulding or sheet metal is the correct route, the DFM note says so — we would rather quote nothing than quote a printed part that cannot compete.
We run four stages. The rest is named in the quotation.
Additive is easy to describe and hard to divide. This is the split we work to, so nobody has to work out later who is responsible when a part arrives out of tolerance.
Stage
Who runs it
What you receive
DFM review
Us
A written note in 24–48 hours: wall thickness, overhangs, support access, assembly clearance, load direction against build orientation, and the machine we intend to run.
Printing, polymer FDM
Us, on our own four machines
Parts from four envelopes up to 1200 × 800 × 1000 mm per part; nozzle up to 525 °C, bed and chamber up to 150 °C held constant.
Support removal and finishing
Us
Supports removed and faces finished to the route agreed at DFM: sanding, bead blasting, vapour smoothing on ABS and PC, tapping, heat-set inserts, painting, bonding, assembly.
First-article inspection
Us
A dimensional report on the declared critical dimensions, plus a cosmetic check against the face standard agreed before the build.
SLS and SLA
Partner, named in the quotation
Quoted per project. The quotation states who produces the parts, and we accept them against the same inspection criteria we apply to our own.
Metal printing
Partner line, named in the quotation
Build, heat treatment and machining sit with the partner. DFM, finishing hand-off and acceptance stay with us.
If an operation is not ours, the quotation says whose it is. An outsourced part is never described as in-house. The polymer line and the metal line share one DFM, inspection and delivery process — the difference is who holds the machine.
The part itself passes through eight steps. Each one can be the reason a dimension moves.
Step
What physically happens
What it fixes — and what it can spoil
01 File check
The STEP is read; open shells, zero-thickness walls and scale are checked. Duty, tolerances and finishing are matched against the geometry.
Fixes the revision that gets printed. A file changed after this point re-opens the DFM.
02 Slicing and orientation
The model is cut into layers at 0.10–0.30 mm and turned on the bed. Orientation sets where supports land and which way a load crosses the layers.
Fixes strength direction and the surface on each face. Change it later and both change.
03 Machine assignment
The part goes to the smallest envelope that holds it, or to the heated-chamber machine if the grade needs one.
Fixes the date, and part of the price.
04 Printing
Bead on bead, layer on layer, inside a chamber held at temperature. Nozzle to 525 °C; bed and chamber to 150 °C.
Fixes the as-built geometry, shrinkage included.
05 Support removal
Supports are cut away at their contact points; witness marks stay on the surface.
Can spoil a face that was in tolerance. The contact side is chosen at slicing for this reason.
06 Finishing
Sanding, bead blasting, vapour smoothing on ABS and PC only, tapping, heat-set inserts, painting, bonding, assembly.
Moves a dimension as well as a surface. A face in tolerance before the last step is not in tolerance after it.
07 Inspection
Declared critical dimensions are measured and reported; cosmetic faces are checked against the standard agreed before the build.
Fixes whether the part ships. The class is ±0.3 mm or ±0.3 %, whichever is greater.
08 Packing
The part is packed to arrive in the condition it was inspected in.
Nothing is measured here. It is the step where a passed part can still be lost.
Prototypes normally run 3–5 working days and small batches 7–12, counted from the point where file, material and finishing are settled — not from the enquiry.
These five cases do not belong on this route.
Each one is a real reason to choose another process. We would rather lose the order at the enquiry than at the first article.
Batch cost inverts the whole calculation.
Above the crossover, the per-part price of printing stops falling while moulding keeps falling. If the annual volume is steady and the geometry is mouldable, a tool pays for itself — and we will point at it rather than print the batch at a higher unit price.
Surface roughness is a process property, not a setting.
Layer texture follows layer height and surface angle, and on a curved or sloped face it cannot be tuned away. Where a Class-A finish is specified, the face is printed oversize and machined, or the part is moulded. Printing alone does not deliver it.
Material certification does not come with the print.
A printed part carries the grade's data sheet, not a part-level certificate. Where the duty requires a certified material, a batch record and a traceable test, the route has to be agreed before the first build — it is not something that can be added at the end.
Tolerance beyond the class is a machining job.
Delivered tolerance is ±0.3 mm or ±0.3 %, whichever is greater, and tightening to ±0.15 mm is a per-feature decision taken after the geometry is checked — never a batch default. A feature that must hold closer than the class is printed with stock and machined.
Long-term weathering is a material question first.
UV, moisture and freeze-thaw change a printed part faster along its layer boundaries than inside the bead. Outdoor duty over years needs a stabilised grade, a protective coating and a test plan; printing a standard grade and hoping is not a specification.
Where a part lands in any of these, we name the process that fits. Where it is useful we make an introduction, but technical negotiation, contract, quality and after-sales stay with that supplier.
Printed parts join conventional processes. They do not replace them.
Most parts we ship are printed and then finished on something else. The joining point is fixed at DFM, because it sets the stock allowance and the datum — decide it after the build and the part has to be printed again.
Print, then machine the faces that mate.
Additive holds shape; it does not hold a bearing seat. Mating, sealing and locating faces are printed with machining stock, then faced, bored or reamed on a CNC. The datum and the allowance go into the DFM note, so the blank arrives with something to cut.
Print the master, cast the small batch in silicone.
When you need more samples than printing justifies and fewer than a tool requires, a printed master goes into a silicone mould and the batch is cast. Appearance and assembly are then judged on the batch, before tooling money is committed.
Printed jigs replace machined fixtures.
A fixture that only has to hold a part for one operation is usually cheaper printed: no drawing release, no machining queue, and a geometry change costs a new file instead of a rework. Where the fixture must hold tolerance for years, it is machined — and we say so.
Where each question is answered next.
The 24 grades, with data per grade
Nine families, one data page each, and side-by-side comparison. Figures are typical values in the process window, not a specification guarantee.
Send the file. The first answer is which process, not which price.
STEP file, quantity, duty, the tolerances that must hold and the finishing. Within 24–48 hours you get the route we would run, the machine, the tolerance class — and the volume at which that route stops paying.
NDA on request. Drawings are used for this project only — never reused, resold or shown to third parties. Published cases stay anonymous: no customer name, no product appearance, no identifying detail. Read the IP commitment →